DIM-L-1.3954
Welding wire DIM L-1.3954
Description:
Material no.: 1.3954
DIN 8556: SG-X 2 CrNiMnMoN 22 17 8 4
EN ISO 14343-A: GZ 22 17 8 4 N L
Non-magnetic, highly alloyed, highly corrosion-resistant
Characteristics:
The N2-alloyed, fully austenitic and non-magnetic solid wire electrode is distinguished by its particularly good resistance to pitting, gap and stress corrosion cracking. Very good low-temperature toughness can be used up to + 350° C or + 400° C for media that do not cause intercrystalline corrosion. Use for seawater desalination plants, centrifuges, bleaching plants and in special shipbuilding, as well as for the welding of cold-steels, e.g. X8Ni9.
Materials:
1.3948 X4CrNiMnMoN19-13-8, 1.3951 X2CrNiMoN22-15, 1.3952 X2CrNiMoN18-14-3, 1.3953 X2CrNiMo18-15, 1.3964 X2CrNiMnMoNNb21-16-5-3, 1.4439 X2CrNiMoN17-13-5
Analysis in %:
C |
Si |
Mn |
Cr |
Ni |
Mo |
N | PREN |
0.02 |
0.63 |
7.3 |
22.2 |
17.7 |
3.7 |
0.23 | 37 |
Mechanical properties of pure weld metal:
pure weld metal | + 20°C |
Tensile strength Rm MPa | 680 (≥ 640) |
Yield strengthRp0.2 MPa | 440 (≥ 430) |
Elongati on A (L0=5d0) % | 32 (≥ 30) |
Impact energy ISO-V KV J +20°C | -196°C | 120 (≥ 70) | (≥ 32) |
- Australia
- Germany
- Denmark
- Switzerland
- Austria
- Argentina
Welding wire DIM L-1.3954
Description:
Material no.: 1.3954
DIN 8556: SG-X 2 CrNiMnMoN 22 17 8 4
EN ISO 14343-A: GZ 22 17 8 4 N L
Non-magnetic, highly alloyed, highly corrosion-resistant
Characteristics:
The N2-alloyed, fully austenitic and non-magnetic solid wire electrode is distinguished by its particularly good resistance to pitting, gap and stress corrosion cracking. Very good low-temperature toughness can be used up to + 350° C or + 400° C for media that do not cause intercrystalline corrosion. Use for seawater desalination plants, centrifuges, bleaching plants and in special shipbuilding, as well as for the welding of cold-steels, e.g. X8Ni9.
Materials:
1.3948 X4CrNiMnMoN19-13-8, 1.3951 X2CrNiMoN22-15, 1.3952 X2CrNiMoN18-14-3, 1.3953 X2CrNiMo18-15, 1.3964 X2CrNiMnMoNNb21-16-5-3, 1.4439 X2CrNiMoN17-13-5
Analysis in %:
C |
Si |
Mn |
Cr |
Ni |
Mo |
N | PREN |
0.02 |
0.63 |
7.3 |
22.2 |
17.7 |
3.7 |
0.23 | 37 |
Mechanical properties of pure weld metal:
pure weld metal | + 20°C |
Tensile strength Rm MPa | 680 (≥ 640) |
Yield strengthRp0.2 MPa | 440 (≥ 430) |
Elongati on A (L0=5d0) % | 32 (≥ 30) |
Impact energy ISO-V KV J +20°C | -196°C | 120 (≥ 70) | (≥ 32) |